1.Anti-foaming and defoaming
1.1 Testing method 0.2% addition in varnish, oscillation 15min, test the density at different time Density is a symbolic measurement of ability of anti-foaming and defoaming. Much more bubbles, lower density. Density value becomes higher with bubbles disappearance.
1.2 Data sheet of density(25℃ g/ml)
1.2.1 Hydroxyl acrylic system
Item |
0min |
5min |
10min |
15min |
Similarproduct |
0.961 |
0.972 |
0.976 |
0.979 |
XOANONS®WE-D912 |
0.964 |
0.974 |
0.977 |
0.979 |
Blank |
0.921 |
0.936 |
0.956 |
0.977 |
1.2.2Short-oilsystem
Item |
0min |
5min |
10min |
15min |
Similarproduct |
1.020 |
1.029 |
1.034 |
1.041 |
XOANONS®WE-D912 |
1.022 |
1.031 |
1.036 |
1.041 |
Blank |
0.890 |
0.939 |
1.011 |
1.040 |
2.Compatibility
System |
Item |
Addition0.1% |
Addition0.15% |
Addition0.2% |
Hydroxylacrylic |
Similarproduct |
5 |
5 |
4 |
XOANONS®WE-D912 |
5 |
4 |
3 |
Short-oilalkyd |
Similarproduct |
5 |
5 |
3 |
XOANONS®WE-D912 |
5 |
4 |
3 |
0=unavailable 5=very effective
3.No side effect Add 0.3% defoaming to varnish, prepare the panel, there’s no shrinkage.
|